USKGLS - 05

USKGLS - 05

0.18MM FINGER UNLOCK HD GLASS

 

Glass: High Aluminum 0.18mm Glass

Glue: 480 ESD high permeability glue

Edge Compression Test: 15-18KG

Water drop angle: 118°

Tempering Time: 5H

Tempering Hardness: 9H

Arc:110 C Falling ball test: 30g/120cm 3times not breaking

Folding degree: 360 /O shape

Oil: Electroplating fingerprint oil , resistant to friction 10,000 times

Bottom plate: 0.5MM, 1:1 PC